1.5920 (case hardened)
Tensile Strength
1500 MPa
Thermal Conductivity
35 W/(m·K)
Elongation
8 %
Chemical Composition
C: 0.18%, Cr: 2%, Ni: 2%, Mn: 0.5%, Si: 0.28%, P: 0.03%, S: 0.03%
Other Names
18CrNi8
DIN 17210
18CN8
18H2N2