1.4542+A
- Tensile Strength
- 1000 MPa
- Thermal Conductivity
- 18 W/(m·K)
- Elongation
- 18 %
- Chemical Composition
- C: 0.07%, Cr: 17%, Ni: 5%, Cu: 5%, Nb + Ta: 0.45%, Mn: 1%, Si: 1%, P: 0.04%, S: 0.03%
Other Names
- X5CrNiCuNb16-4
- 17-4 PH
- AISI 630
- UNS S17400
Material Description
Lorem ipsum