1.4501
- Tensile Strength
- 900 MPa
- Thermal Conductivity
- 15 W/(m·K)
- Elongation
- 20 %
- Chemical Composition
- C: 0.03%, Cr: 26%, Ni: 8%, Mo: 4%, W: 1%, Cu: 1%, Si: 1%, Mn: 1%, N: 0.3%, P: 0.035%, S: 0.015%
Other Names
- X2CrNiMiCuWN25-7-4
- UNS S32760
- F55
- Alloy 100 Super-Duplex
- Zeron 100
Material Description
Lorem ipsum