1.3292 65HRC+
- Tensile Strength
- 2500 MPa
- Thermal Conductivity
- 12 W/(m·K)
- Elongation
- 1.5 %
- Chemical Composition
- C: 2.4%, Co: 11%, V: 7.3%, W: 7.3%, Mo: 6.7%, Cr: 4.5%, Si: 0.7%, Mn: 0.4%, P: 0.05%, S: 0.03%
Other Names
- ASP2060
- Vanadis 60 SuperClean
- SPM60